Effects of aging and light-curing unit type on the volume and internal porosity of bulk-fill resin composite restoration
dc.contributor.author | Al-Zain, Afnan O. | pt_BR |
dc.contributor.author | Alboloshi , Elaf A. | pt_BR |
dc.contributor.author | Amir, Walaa A. | pt_BR |
dc.contributor.author | Alghilan, Maryam A. | pt_BR |
dc.contributor.author | Münchow, Eliseu Aldrighi | pt_BR |
dc.date.accessioned | 2022-07-15T04:48:40Z | pt_BR |
dc.date.issued | 2022 | pt_BR |
dc.identifier.issn | 1013-9052 | pt_BR |
dc.identifier.uri | http://hdl.handle.net/10183/242581 | pt_BR |
dc.description.abstract | This study explores the effects of aging (thermal cycling and cyclic loading–TC/CL) and different light-curing unit (LCU) types on the volume characteristics and internal porosity of a bulk-fill resin-based composite restoration. Occlusal cavities (4 × 4 × 3 mm) were prepared on extracted human molars (n = 5). Tetric N-Bond Universal was applied, and the cavities were restored using Tetric-N-Ceram Bulk Fill. Photoactivation was performed using a quartz-tungsten halogen (QTH) or a multiple-emission peak light-emitting diode (MLED). Digital images for all restorations were obtained using microcomputed tomography (micro-CT) before (baseline) and after (post-aging) TC/CL (5,000 TC cycles in 5–55 °C baths and a dwell time of 30 s followed by 10,000 sinusoidal CL load cycles in an Instron B3000 at 2 Hz and 10–110 N) and storage (37 °C) for three months. For the micro-CT analysis, three-dimensional images were used to determine the restoration volume and internal porosity. Data were analyzed using a two-way ANOVA and Tukey’s test (p < 0.05). Restorations photoactivated with QTH exhibited a higher object volume than the LED group at baseline and in post-aging conditions without any significant differences in the other evaluated characteristics. All volume/porosity characteristics increased considerably after TC/CL aging, except for the object volume of the QTH group and the closed porosity of the MLED group. The change in all the volume/porosity characteristics between both LCU groups after TC/CL were not significantly different. Thus, the aging process simulated herein increased the volume and porosity characteristics of the bulk-fill restoration, and no significant differences were obtained between the QTH and MLED equipment. | en |
dc.format.mimetype | application/pdf | pt_BR |
dc.language.iso | eng | pt_BR |
dc.relation.ispartof | Saudi Dental Journal. Riyadh. Vol.34, no. 3 (mar. 2022), p.243-248 | pt_BR |
dc.rights | Open Access | en |
dc.subject | Bulk-filling technique | en |
dc.subject | Resinas compostas : Fotopolimerizaveis | pt_BR |
dc.subject | Quartz-tungsten-halogen | en |
dc.subject | Microtomografia por raio-x | pt_BR |
dc.subject | Light-emitting diode | en |
dc.subject | Micro-computed tomography | en |
dc.subject | Thermal cycling | en |
dc.subject | Cyclic loading | en |
dc.title | Effects of aging and light-curing unit type on the volume and internal porosity of bulk-fill resin composite restoration | pt_BR |
dc.type | Artigo de periódico | pt_BR |
dc.identifier.nrb | 001140895 | pt_BR |
dc.type.origin | Estrangeiro | pt_BR |
Ficheros en el ítem
Este ítem está licenciado en la Creative Commons License
-
Artículos de Periódicos (40917)Ciencias de la Salud (10934)