dc.description.abstractO objetivo do presente estudo foi formular um adesivo ortodôntico experimental com a incorporação de nanotubos de nitreto de boro (BNNTs) e brometo de alquil trimetil amônio (ATAB) como carga, e caracterizar conforme suas propriedades. Foi formulada uma resina base, composta por 75% de Bis-GMA e 25% TEGDMA, 1% mol de CQ, EDAB, DPIH, 0,01% de BHT em peso, além de 5% de sílica coloidal. Foi adicionado à resina base 0,1% BNNT (GBNNT); 0,1% ATAB (GATAB) e 0,2% BNNT/ATAB (GBNNT/ATAB), e um grupo permaneceu sem adição de carga o qual foi usado como grupo controle (GCtrl). Os grupos foram avaliados através dos testes de resistência de união ao cisalhamento (n=15), ação antimicrobiana (n=3), grau de conversão (n=3), ângulo de contato e energia livre de superfície (n=5), amolecimento em solvente (n=5), deposição mineral (n=5) e citotoxicidade (n=3). Os dados foram analisados utilizando teste t-student pareado para amolecimento em solvente e ANOVA de uma via para os outros testes, havendo diferenças entre os grupos, foi aplicado o teste de comparações múltiplas de Tukey. O nível de significância foi de 5%. Todos os grupos alcançaram valores de conversão acima de 50% e viabilidade celular superior a 90%. Os adesivos GBNNT (12,74±7,32) e GATAB (13,67±8,28) exibiram redução do amolecimento no solvente em comparação com o adesivo GCtrl. O valor médio da energia livre de superfície foi diminuído (p<0,05) no adesivo GBNNT (44,86±3,41). Uma redução significativa no crescimento bacteriano foi observada com o adesivo GBNNT/ATAB (p<0,05). Todos os grupos foram semelhantes nas avaliações de resistência ao cisalhamento (p>0,05). Teste de deposição mineral revelaram deposição de fosfato nos grupos GBNNT, GATAB e GBNNT/ATAB após 14 e 28 dias. A adição de 0,2% de BNNT/ATAB a um adesivo ortodôntico experimental é capaz de inibir o crescimento bacteriano e induzir deposição mineral sem afetar as propriedades do material.pt_BR
dc.description.abstractThe aim of the present study was to formulate an experimental orthodontic adhesive with the incorporation of boron nitride nanotubes (BNNTs) and alkyl trimethyl ammonium bromide (ATAB) as a filler, and characterize according to its properties. A base resin composed of 75% Bis-GMA and 25% TEGDMA, 1 mol% of CQ, EDAB, DPIH, 0.01% BHT by weight, and 5% of colloidal silica was formulated. 0.1% BNNT was added to the base resin (GBNNT); 0.1% ATAB (GATAB) and 0.2% BNNT/ATAB (GBNNT/ATAB), and one group remained unfilled, which was used as the control group (GCtrl). The groups were evaluated through shear bond strength tests (n = 15), antimicrobial action (n = 3), degree of conversion (n = 3), contact angle and free surface energy (n = 5), softening in solvent (n = 5), mineral deposition (n = 5) and cytotoxicity (n = 3). The data were analyzed using paired t-student test for solvent softening and one-way ANOVA for the other tests. There were differences between groups, Tukey's multiple comparisons test was applied. The level of significance was 5%. All groups achieved conversion values above 50% and cell viability greater than 90%. GBNNT (12.74 ± 7.32) and GATAB (13.67 ± 8.28) adhesives exhibited reduced softening in solvent compared to GCtrl adhesive. The mean free surface energy was decreased (p <0.05) in GBNNT adhesive (44.86 ± 3.41). A significant reduction in bacterial growth was observed with GBNNT/ATAB adhesive (p <0.05). All groups were similar in the shear strength ratings (p>0,05). Mineral deposition test revealed phosphate deposition in the GBNNT, GATAB and GBNNT/ATAB groups after 14 and 28 days. The addition of 0.2% of BNNT/ATAB to an experimental orthodontic adhesive is able to inhibit bacterial growth and induce mineral deposition without affecting the properties of the material.en
dc.format.mimetypeapplication/pdfpt_BR
dc.language.isoporpt_BR
dc.rightsOpen Accessen
dc.subjectCimentos dentáriospt_BR
dc.subjectOrthodontic adhesiveen
dc.subjectOrtodontiapt_BR
dc.subjectDental cariesen
dc.subjectMateriais odontológicospt_BR
dc.subjectNanotubesen
dc.subjectNanotubospt_BR
dc.titleNanotubos de nitreto de boro e brometo de alquil trimetil amônio como carga em um adesivo ortodôntico experimentalpt_BR
dc.typeDissertaçãopt_BR
dc.identifier.nrb001074681pt_BR
dc.degree.grantorUniversidade Federal do Rio Grande do Sulpt_BR
dc.degree.departmentFaculdade de Odontologiapt_BR
dc.degree.programPrograma de Pós-Graduação em Odontologiapt_BR
dc.degree.localPorto Alegre, BR-RSpt_BR
dc.degree.date2018pt_BR
dc.degree.levelmestradopt_BR


Ficheros en el ítem

Thumbnail
   

Este ítem está licenciado en la Creative Commons License

Mostrar el registro sencillo del ítem