Show simple item record

dc.contributor.authorOgliari, Fabricio Aulopt_BR
dc.contributor.authorCollares, Fabrício Mezzomopt_BR
dc.contributor.authorCampregher, Ulisses Bastospt_BR
dc.contributor.authorFortes, Carmen Beatriz Borgespt_BR
dc.contributor.authorSamuel, Susana Maria Wernerpt_BR
dc.date.accessioned2020-12-28T04:15:23Zpt_BR
dc.date.issued2004pt_BR
dc.identifier.issn0566-1854pt_BR
dc.identifier.urihttp://hdl.handle.net/10183/216921pt_BR
dc.description.abstractVárias pesquisas têm sido feitas co a finalidade de otimizar os métodos de polierização das resinas acrílicas. Dentre as descobertas inclui-se a utilização da energia de microondas. Para as resinas acrílicas nacionais, os fabricantes preconizam um ciclo de polimerização alternado de 3 minutos em uma potência de 4OOW, 4 minutos a OW e mais 3 minutos a 800W. Riscando simplificar ainda mais o processo de polimerização das resinas acrílicas, surgiu a proposta de um ciclo alternativo de 3 minutos a 500W. Sendo assim, o objetivo deste trabalho é analisar a eficácia deste novo ciclo através do ensaio de resistência flexural, de acordo com a especificação n° 1567 da ISO, que requer um valor mínino dc 65MPa. Foram confeccionados 10 corpos de prova da resina acrílica termopolimerizável em microondas da marcas Onda CryI, divididos em dois grupos: o grupo controle (C), polimerizado de acordo com as orientações do fabricante e o grupo experimental (E), polimerizado por 3 minutos com 500W de potência. A partir dos testes realizados em uma máquina de ensaios obteve-se os seguintes resultados médios de resistência flexural em Mpa e respectivos desvios-padrão: C= 83,85 ±6,51 e E= 89,72 ± 6,84. Com base nos resultados é Lícito concluir que em relação à resistência flexural, a resina polimerizável em microondas Onda Cryl, pode ser polimerizada no ciclo reduzido de 3 minutos a 500W, uma vez que os resultados obtidos no presente estudo atenderam à expecificação nº 3 567 da ISO.pt_BR
dc.description.abstractSeveral researches have been done to optimize the methods of acrylic resin cure. Among the discoveries, the utilization of the microwave oven energy is in included. For the Brazilian acrylic resins, the produ cers commend a cure cycles alternated from 3 minutes at 400W potency, 4 minutes at OW and 3 minutes at 800W. Trying to simplify even more the acrylic resin cure. process, an alternative 3 minutes at 50OW cycle is presented. The purpose of this study is to analyze his new cicle efficacy , through the flexural strength test, in agreement with the ISO specification number 1567, which requests a minimum value of 65 Mpa. Ten specimens of acrylic resin therm-cured in the microwave oven of Onda Crylâ brand, were made. They’re divided in two groups: the control group (C), cured agreement to the producers orientation and the experimental group (E), cured for 3 minutes at 500W of potency. The tests were made in a tests machines and the following medium results of flexural strength in Mpa were obtained: C 83,85 (±6,51) and E 89,72 (±6,84). With the result it's licit to concluded that with regard to the flexural strength, the microwave cured resin Onda Crylâ, can be cured in the reduced cycle from 3 minutes at 500W, once the results obtained l with the present study attend to the ISO specification number 1567.en
dc.format.mimetypeapplication/pdfpt_BR
dc.language.isoporpt_BR
dc.relation.ispartofRevista da Faculdade de Odontologia de Porto Alegre. Porto Alegre. Vol. 45, n. 2 (dez. 2004), p. 54-56pt_BR
dc.rightsOpen Accessen
dc.subjectMicrowave ovenen
dc.subjectMateriais odontologicos : Avaliacaopt_BR
dc.subjectResinas acrílicaspt_BR
dc.subjectAcrylic resinen
dc.subjectFlexural strenghten
dc.titleResistência flexural de resina acrílica polimerizável em microondaspt_BR
dc.title.alternativeFlexural strenght of acrylic resin rured by microwave oven en
dc.typeArtigo de periódicopt_BR
dc.identifier.nrb000474819pt_BR
dc.type.originNacionalpt_BR


Files in this item

Thumbnail
   

This item is licensed under a Creative Commons License

Show simple item record