Mostrar registro simples

dc.contributor.authorFigueiredo, Camila Araújo dept_BR
dc.contributor.authorCatafesta, Jadnapt_BR
dc.contributor.authorZorzi, Janete Eunicept_BR
dc.contributor.authorSouza, Leonardo Salvadorpt_BR
dc.contributor.authorBaumvol, Israel Jacob Rabinpt_BR
dc.contributor.authorGallas, Marcia Russmanpt_BR
dc.contributor.authorJornada, Joao Alziro Herz dapt_BR
dc.contributor.authorPerottoni, Claudio Antoniopt_BR
dc.date.accessioned2014-10-14T02:12:59Zpt_BR
dc.date.issued2007pt_BR
dc.identifier.issn1098-0121pt_BR
dc.identifier.urihttp://hdl.handle.net/10183/104512pt_BR
dc.description.abstractThe structure of [upsilon]-ZrW2O8 has been optimized at zero pressure and also at V/V0=0.97 by means of density functional theory calculations using the B3LYP functional. As previously found for [upsilon]-ZrW2O8, tungsten polyhedra are stiffer than zirconium octahedra in -ZrW2O8. However, contrary to what has been found for [upsilon]-ZrW2O8, all first coordination polyhedra in the phase are less compressible than the unit cell. Volume reduction in [upsilon]-ZrW2O8 is, thus, mainly accomplished by polyhedral tilting. Upon pressure increase, the distance between the terminal oxygen and W atoms from the nearest polyhedra decreases by as much as 3.66% for the pair O101-W6 . Accordingly, a further reduction in the zirconium tungstate molar volume with the high-pressure transition to the amorphous phase should bring several oxygen atoms within the threshold of bond formation to W. O 1s photoelectron spectra provide further experimental evidence on the formation of additional W-O bonds in amorphous zirconium tungstate. These new W-O bonds should enable the metastable retention of the amorphous phase upon pressure release.en
dc.format.mimetypeapplication/pdf
dc.language.isoengpt_BR
dc.relation.ispartofPhysical review. B, Condensed matter and materials physics. Woodbury. Vol. 76, no. 18 (Nov. 2007), 184201 7p.pt_BR
dc.rightsOpen Accessen
dc.subjectFísica da matéria condensadapt_BR
dc.titleCompression mechanism and pressure-induced amorphization of [upsilon]-ZrW/sub 2/O/sub 8/pt_BR
dc.typeArtigo de periódicopt_BR
dc.identifier.nrb000624129pt_BR
dc.type.originEstrangeiropt_BR


Thumbnail
   

Este item está licenciado na Creative Commons License

Mostrar registro simples